Temper | Annealed | |
---|---|---|
Tensile Rm | 76 | ksi (min) |
Tensile Rm | 517 | MPa (min) |
R.p. 0.2% Yield | 31 | ksi (min) |
R.p. 0.2% Yield | 207 | MPa (min) |
Elongation (2” or 4D gl) | 40 | % (min) |
Element | Min | Max |
---|---|---|
C | - | 0.25 |
Mn | - | 2 |
Ni | 19 | 22 |
Cr | 24 | 26 |
Si | - | 1.5 |
P | - | 0.045 |
S | - | 0.03 |
Temper | Annealed | |
---|---|---|
Tensile Rm | 76 | ksi (min) |
Tensile Rm | 517 | MPa (min) |
R.p. 0.2% Yield | 31 | ksi (min) |
R.p. 0.2% Yield | 207 | MPa (min) |
Elongation (2” or 4D gl) | 40 | % (min) |
Element | Min | Max |
---|---|---|
C | - | 0.25 |
Mn | - | 2 |
Ni | 19 | 22 |
Cr | 24 | 26 |
Si | - | 1.5 |
P | - | 0.045 |
S | - | 0.03 |