Incoloy 926 Characteristic: 1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
2.In practice, effective in resistance of chloride stress corrosion cracking.
3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
6.With a certification of applied in manufacturing-related? pressure vessel (VdTUV-196~400℃ and ASME )
Incoloy 926 Chemical composition: Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | Mo | N | Ti | P | S |
926 | Min. | 24 | 19 | Balance | | | | 0.5 | 6.0 | 0.15 | 0.6 | | |
Max. | 26 | 21 | 0.02 | 2 | 0.5 | 1.5 | 7.0 | 0.25 | 1.2 | 0.03 | 0.01 |
Incoloy 926 Physical properties: Density | 8.1 g/cm3 |
Melting point | 1320-1390 ℃ |
Incoloy 926 Alloy Minimum Mechanical properties in the room temperature: Alloy state | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
926 | 650 | 295 | 35 |
Incoloy 926 Characteristic:
1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
2.In practice, effective in resistance of chloride stress corrosion cracking.
3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
6.With a certification of applied in manufacturing-related? pressure vessel (VdTUV-196~400℃ and ASME )
Incoloy 926 Chemical composition: Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | Mo | N | Ti | P | S |
926 | Min. | 24 | 19 | Balance | | | | 0.5 | 6.0 | 0.15 | 0.6 | | |
Max. | 26 | 21 | 0.02 | 2 | 0.5 | 1.5 | 7.0 | 0.25 | 1.2 | 0.03 | 0.01 |
Incoloy 926 Physical properties: Density | 8.1 g/cm3 |
Melting point | 1320-1390 ℃ |
Incoloy 926 Alloy Minimum Mechanical properties in the room temperature: Alloy state | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
926 | 650 | 295 | 35 |