Alloy | % | Ni | Cr | Fe | Nb | Co | C | Mn | Si | S | Cu | Al | Ti |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Inconel X-750 | Min. | | 14 | 5.0 | 0.7 | | | | | | | 0.4 | 2.25 |
Max. | 70 | 17 | 9.0 | 1.2 | 1.00 | 0.08 | 1.00 | 0.5 | 0.01 | 0.5 | 1.0 | 2.75 |
Density | 8.28 g/cm3 |
Melting range | 1393-1427℃ |
Alloy | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % | Brinell hardness HB |
Solution treatment | 1267 | 868 | 25 | ≤400 |
Alloy | % | Ni | Cr | Fe | Nb | Co | C | Mn | Si | S | Cu | Al | Ti |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Inconel X-750 | Min. | | 14 | 5.0 | 0.7 | | | | | | | 0.4 | 2.25 |
Max. | 70 | 17 | 9.0 | 1.2 | 1.00 | 0.08 | 1.00 | 0.5 | 0.01 | 0.5 | 1.0 | 2.75 |
Density | 8.28 g/cm3 |
Melting range | 1393-1427℃ |
Alloy | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % | Brinell hardness HB |
Solution treatment | 1267 | 868 | 25 | ≤400 |