Alloy | % | Ni | Cu | Al | Ti | Fe | Mn | S | C | Si |
---|---|---|---|---|---|---|---|---|---|---|
Monle K500 | Min. | 63 | 27.0 | 2.30 | 0.35 | | | | | |
Max. | | 33.0 | 3.15 | 0.85 | 2.0 | 1.5 | 0.01 | 0.25 | 0.5 |
Density | 8.44 g/cm3 |
Melting point | 1315-1350℃ |
Status | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
Monel K500 | 1100 | 790 | 20 |
Bar | Rod |
---|---|
AMS 4676 | AMS 4676 |
Alloy | % | Ni | Cu | Al | Ti | Fe | Mn | S | C | Si |
---|---|---|---|---|---|---|---|---|---|---|
Monle K500 | Min. | 63 | 27.0 | 2.30 | 0.35 | | | | | |
Max. | | 33.0 | 3.15 | 0.85 | 2.0 | 1.5 | 0.01 | 0.25 | 0.5 |
Density | 8.44 g/cm3 |
Melting point | 1315-1350℃ |
Status | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
Monel K500 | 1100 | 790 | 20 |
Bar | Rod |
---|---|
AMS 4676 | AMS 4676 |